by mikeypep » Fri Apr 04, 2008 10:38 am
Yup, yup and yuppers. Krylon Fusion and Rustoleum Plastics Paint really
work. I did find that surface prep is critical. I used some silicone
based wax on my KLR plastics and get a lot of fisheye, plus poor
adhesion but surfaces I didn't wax are h olding up very well.
--- In
DSN_KLR650@yahoogroups.com, "Andrus Chesley"
wrote:
>
> Wayne,
> In my experience. If I don't want paint on something and it gets
there
> anyway. I can't get it off never!. If I want it there, It won't
> stick.

.. Kidding a little. Just light sand and a good quality
> paint will work. Think they even have some for plastic. I picked up
a
> can of Flat Black a few years ago for some plastic on my bike and
just
> light sand , clean and spray. Can you believe, it's still there.

>
> Andy in Louisiana
> A14 KLR K6 DLK
>